Wide range of indications, suitable for anterior restorations.

The transition between layers ensures efficient production of natural-looking restorations.


ADVANTAGES

✔ Stable in work, easy to mill

✔ Efficient process, only requires glaze

✔ Layer transition that guarantees a natural and efficient aesthetic result

FEATURES

CUBIC-ML

Monoclinic phase content:
<15%

Sintering density:
6.06 ± 0.01 g/cm³

Sintering temperature:
1450 °C

Flexural strength:
600 MPa

Translucency:
>49%

Solid-ML

Monoclinic phase content:
<15%

Sintering density:
6.07 ± 0.01 g/cm³

Sintering temperature:
1530 °C

Flexural strength:
1100 MPa

Translucency:
<43%

Vitality-ML

Monoclinic phase content:
<15%

Sintering density:
6.08 ± 0.01 g/cm³

Sintering temperature:
1530 °C

Flexural strength:
900 MPa

Translucency:
<46%

Want to know more about this and other products?

Contact us.

Cookies
Cookies are used to access and store information on your device in order to provide personalised content and advertisements based on your data.
By selecting ‘I agree,’ you consent to the use of cookies. You may decline or withdraw your consent by selecting ‘Manage settings.’
| |